Magnus Metal wants to revamp the 4,000-year-old way metal parts are made

techcrunch.com
submitted
a year ago
byrss-bot bottotechnology

Summary

In the casting machine, metal is melted and dripped into the ceramic base. Once a layer is complete, more metal is added. Each subsequent layer melts the previous one, ensuring the layers are bonded. Magnus Metals has raised $74 million in funding. The company uses a layer-by-layer method to create the bases, unlike molds for sand casting.